Slata Babhta Cruach Éadrom
Is cruach ísealcharbóin é cruach éadrom le cion carbóin 0.15% ~ 0.30% agus cion mangainéise nach mó ná 0.75%. Is cineál cruach carbóin é cruach ísealcharbóin.
Tá neart íseal, cruas íseal, agus bog mar thréith ag cruach éadrom. Áiríonn sé an chuid is mó de ghnáthchruach struchtúrach carbóin agus roinnt cruach struchtúrach carbóin ardchaighdeáin. Úsáidtear an chuid is mó díobh le haghaidh páirteanna struchtúracha innealtóireachta gan chóireáil teasa, agus úsáidtear cuid acu freisin le haghaidh páirteanna meicniúla a bhfuil cóireáil teasa orthu a dteastaíonn friotaíocht caitheamh uathu, mar shampla carburizing.
Meáchan Barraí Babhta Cruach Carbóin
| MÉID IN ORCHAÍ | Babhta | Cearnóg | OCTAGÓIN | HEXAGON | MÉID IN ORCHAÍ | Babhta | Cearnóg | OCTAGÓIN | HEXAGON |
| 1/16 | .010 | .013 | .011 | .012 | 11/16 | 1.262 | 1.607 | 1.333 | 1.392 |
| 5/64 | .017 | .022 | .018 | .019 | 45/64 | 1.320 | 1.681 | 1.394 | 1.456 |
| 3/32 | .023 | .029 | .024 | .025 | 23/32 | 1.380 | 1.756 | 1.487 | 1.521 |
| 7/64 | .031 | .039 | .033 | .034 | 47/64 | 1.440 | 1.834 | 1.521 | 1.588 |
| 1/8 | .042 | .053 | .044 | .046 | 3/4 | 1.502 | 1.913 | 1.586 | 1.656 |
| 9/64 | .053 | .067 | .056 | .058 | 25/32 | 1.630 | 2.075 | 1.721 | 1.797 |
| 5/32 | .065 | .083 | .069 | .072 | 13/16 | 1.763 | 2.245 | 1.862 | 1.944 |
| 11/64 | .079 | .100 | .083 | .087 | 27/32 | 1.901 | 2.421 | 2.008 | 2.096 |
| 3/16 | .094 | .120 | .099 | .104 | 7/8 | 2.045 | 2.603 | 2.159 | 2.254 |
| 13/64 | .110 | .140 | .116 | .121 | 29/32 | 2.193 | 2.792 | 2.316 | 2.418 |
| 7/32 | .128 | .163 | .135 | .141 | 15/16 | 2.347 | 2.988 | 2.479 | 2.588 |
| 15/64 | .147 | .187 | .155 | .162 | 31/32 | 2.506 | 3.191 | 2.646 | 2.763 |
| 1/4 | .167 | .213 | .176 | .184 | 1 | 2.670 | 3.400 | 2.820 | 2.945 |
| 17/64 | .188 | .240 | .199 | .207 | 1-1/16 | 3.015 | 3.838 | 3.183 | 3.324 |
| 9/32 | .211 | .269 | .223 | .233 | 1-1/8 | 3.380 | 4.303 | 3.569 | 3.727 |
| 19/64 | .235 | .300 | .248 | .259 | 1-3/16 | 3.766 | 4.795 | 3.977 | 4.152 |
| 5/16 | .261 | .332 | .275 | .288 | 1-1/4 | 4.172 | 5.313 | 4.407 | 4.601 |
| 21/64 | .288 | .360 | .304 | .318 | 1-5/16 | 4.600 | 5.857 | 4.858 | 5.072 |
| 11/32 | .316 | .402 | .334 | .348 | 1-3/8 | 5.049 | 6.428 | 5.332 | 5.567 |
| 23/64 | .345 | .439 | .364 | .381 | 1-7/16 | 5.518 | 7.026 | 5.827 | 6.085 |
| 3/8 | .376 | .478 | .397 | .414 | 1-1/2 | 6.008 | 7.650 | 6.345 | 6.625 |
| 25/64 | .408 | .519 | .431 | .450 | 1-9/16 | 6.519 | 8.301 | 6.885 | 7.189 |
| 13/32 | .441 | .561 | .466 | .486 | 1-5/8 | 7.051 | 8.978 | 7.446 | 7.775 |
| 27/64 | .475 | .605 | .502 | .524 | 1-11/16 | 7.604 | 9.682 | 8.030 | 8.385 |
| 7/16 | .511 | .651 | .540 | .564 | 1-3/4 | 8.178 | 10.41 | 8.634 | 9.018 |
| 29/64 | .548 | .698 | .579 | .604 | 1-13/16 | 8.773 | 11.17 | 9.265 | 9.673 |
| 15/32 | .587 | .747 | .620 | .647 | 1-7/8 | 9.388 | 11.95 | 9.911 | 10.35 |
| 31/64 | .627 | .798 | .662 | .692 | 1-15/16 | 10.02 | 12.76 | 10.58 | 11.05 |
| 1/2 | .668 | .850 | .705 | .736 | 2 | 10.68 | 13.60 | 11.28 | 11.78 |
| 33/64 | .710 | .904 | .750 | .783 | 2-1/16 | 11.36 | 14.46 | 11.99 | 12.53 |
| 17/32 | .754 | .960 | .796 | .831 | 2-1/8 | 12.06 | 15.35 | 12.73 | 13.30 |
| 35/64 | .799 | 1.017 | .844 | .881 | 2-3/16 | 12.78 | 16.27 | 13.49 | 14.09 |
| 9/16 | .845 | 1.076 | .892 | .932 | 2-1/4 | 13.52 | 17.21 | 14.27 | 14.91 |
| 37/64 | .893 | 1.136 | .943 | .985 | 2-5/16 | 14.28 | 18.18 | 15.08 | 15.75 |
| 19/32 | .941 | 1.199 | .994 | 1.038 | 2-3/8 | 15.06 | 19.18 | 15.91 | 16.61 |
| 39/64 | .992 | 1.263 | 1.048 | 1.094 | 2-7/16 | 15.87 | 20.20 | 16.75 | 17.49 |
| 5/8 | 1.043 | 1.328 | 1.102 | 1.150 | 2-1/2 | 16.69 | 21.25 | 17.62 | 18.40 |
| 41/64 | 1.096 | 1.395 | 1.207 | 1.209 | 2-9/16 | 17.53 | 22.33 | 18.52 | 19.34 |
| 21/32 | 1.150 | 1.464 | 1.214 | 1.268 | 2-5/8 | 18.40 | 23.43 | 19.43 | 20.29 |
| 43/64 | 1.205 | 1.535 | 1.272 | 1.329 | 2-11/16 | 19.29 | 24.56 | 20.37 | 21.27 |
babhta cruach éadrom Sonraí Táirgí
I gcomparáid le steels meánmhéide agus ardcharbóin, tá foirmiúlacht fuar maith ag cruach éadrom agus is féidir é a fhoirmiú fuar trí chreimeadh, lúbadh agus stampáil. Tá úsáid cruach éadrom teoranta ag a neart íseal. Is féidir neart na cruach a fheabhsú go mór trí ábhar mangainéise cruach carbóin a mhéadú go cuí agus riandúile cóimhiotail a chur leis, mar shampla vanadium, tíotáiniam agus niobium. Má laghdaítear cion carbóin an chruach agus má chuirtear méideanna beaga d’eilimintí foirmithe alúmanaim, bórón agus chomhdhúile leis, is féidir bainít ultra-charbóin íseal a fháil, a bhfuil ard-neart aige agus a chothaíonn plaisteacht agus cruas maith.
cruach carbóin slat stoc Táirgí íomhá


Grianghraf foirne grúpa GNEE

Cuairt chustaiméirí grúpa GNEE

Glacann GNEE Group páirt i dtaispeántais chruach eachtrach

Ráthaímid cáilíocht agus cainníocht na Slata Babhta Cruach Éadrom. Más mian leat tuilleadh eolais a fháil, déan teagmháil linn!
Clibeanna Te: slata bhabhta cruach éadrom, monaróirí slata bhabhta cruach éadrom tSín, soláthraithe, monarcha