Barra Babhta Cruach Alloy Q345


Is cineál ábhar cruach é slat cruach bhabhta Q345. Is cruach cóimhiotail íseal é (C<0.2%), widely used in construction, bridges, vehicles, ships, pressure vessels, etc. Q stands for the yield strength of the material, followed by 345, which means the yield value of the material, in the range of 345 MPa. And with the increase of the thickness of the material will make its yield value decreases.

 

Tá airíonna meicniúla cuimsitheacha barra bhabhta cruach soladach Q345 go maith, tá feidhmíocht teocht íseal fós ar fáil, tá plaisteacht agus weldability maith, a úsáidtear mar choimeádáin brú íseal agus meánmhéide, umair, feithiclí, craenacha, innealra mianadóireachta, stáisiúin chumhachta, droichid agus struchtúir eile faoi réir ualaí dinimiciúla, páirteanna meicniúla, struchtúir tógála, páirteanna struchtúracha miotail ghinearálta, úsáid stáit rollta te nó normalaithe go maith, is féidir iad a úsáid le haghaidh réimse fuar de na réigiúin éagsúla.

 

 
q345 comhdhéanamh ceimiceach cruach barra bhabhta soladach

 

Caighdeán Cruach Grád Cruach Comhdhéanamh Ceimiceach
C Níos lú ná nó cothrom le Mn Si Níos lú ná nó cothrom le P Níos lú ná nó cothrom le S Níos lú ná nó cothrom le V Nb Ti Al Níos mó ná nó cothrom le
Q345 A 0.20 1.00~1.60 0.55 0.045 0.045 0.02~0.15 0.015~0.060 0.20 -
B 0.20 1.00~1.60 0.55 0.040 0.040 0.02~0.15 0.015~0.060 0.20 -
C 0.20 1.00~1.60 0.55 0.035 0.035 0.02~0.15 0.015~0.060 0.20 0.015
D 0.20 1.00~1.60 0.55 0.030 0.030 0.02~0.15 0.015~0.060 0.20 0.015
E 0.20 1.00~1.60 0.55 0.025 0.025 0.02~0.15 0.015~0.060 0.20

0.015

 

 
maoin mheicniúil cruach stoic bhabhta q345

 

Caighdeán Cruach Grád Cruach Mpa Neart Toradh Léarscáil Neart Teanntachta Fadú %
Q345 A 345 470~630 21
B 345 470~630 21
C 345 470~630 22
D 345 470~630 22
E 345 470~630 22

 

 
íomhá stoic bhabhta Táirgí miotail

 

China round stock steel Manufacturers

 

 
Grianghraf foirne grúpa GNEE

 

China structural angle producers

 

 
Cuairt chustaiméirí grúpa GNEE

 

China structural steel angle makers

 

 
Ghlac GNEE Group páirt sa taispeántas Indinéisis

 

China angle steel beam Factory

Tá seirbhís tar éis díolacháin den scoth againn. Má tá aon cheist agat faoi Q345 Alloy Steel Babhta Bar, is féidir leat teagmháil a dhéanamh linn agus cuirfimid freagra chugat laistigh de dhá uair an chloig.

 

Clibeanna Te: barra bhabhta cruach cóimhiotail q345, monaróirí barra bhabhta cruach cóimhiotail tSín q345, soláthraithe, monarcha