Comparáid Idirnáisiúnta de Ghráid Cruach le haghaidh Coirí agus Soithí Brú

Déanann an treoir chuimsitheach tras-tagartha seo gráid choibhéiseacha coire agus cruach soithí brú a léarscáiliú thar mórchaighdeáin idirnáisiúnta, lena n-áirítear ASTM, EN, JIS, GB, agus ISO.

 

Cuid 1: Tras-Tagairt do Phlátaí Cruach (Caighdeán GB 713)

An tSín (GB/YB) SAM (ASTM) an tSeapáin (JIS) An Ghearmáin/RA/An Fhrainc (DIN/BS/NF EN) Rúis (GOST) ISO
Q245R(20g, 20R roimhe seo) A414/A414M Gr. D (JIS G3124) SEV 25 S235JR (1.0038), S235J0 (1.0114), S235J2 (1.0117) Ст3кп P235GH
Q345R(16Mng, 19Mng, 16MnR roimhe seo) A737/A737M Gr. b (JIS G3124) SEV 345 S355JR (1.0045), S355J0 (1.0553), S355J2 (1.0577), S355K2 (1.0596) 17C, 15XCHД P355GH
Q370R(15MnNbR roimhe seo) A572/A572M Gr. 50 (345) (JIS G3115) SPV 355 S355JR (1.0045), S355J0 (1.0553), S355J2 (1.0577), S355K2 (1.0596) 10Г2Б P355GH
18MnMoNbR A735/A735M Gr. 1 (JIS G3115) SPV410 - - -
13MnNiMoR(Roimhe seo 13MnNiCrMoNbg, 13MnNiMoNbR) A738/A738M Gr. b - - - 15NiCuMoNb 5-6-4
15CrMoR(15CrMog roimhe seo) A387/A387M Gr. 12 (K11757) (JIS G4109) SCMV2 18CrMo4 15XM 13CrMo4-5 (Seachadadh mar 14CrMo4-5 in aghaidh an ASME)
14Cr1MoR A387/A387M Gr. 11 (K11789) (JIS G4109) SCMV3 18CrMo4 15XM 13CrMoSi5-5 (Seachadadh mar 14CrMoSi5-6 in aghaidh an ASME)
12Cr2Mo1R A387/A387M Gr. 22 (K21590) (JIS G4109) SCMV4 - - 10CrMo9-10 (Seachadadh mar 13CrMo9-10 nó 14CrMo9-10 in aghaidh an ASME)
12Cr1MoVR(12Cr1MoVg roimhe seo) - - - - -

 

Cuid 2: Feadáin Cruach Gan uaim le haghaidh Coirí Brú Ard-- (Caighdeán GB 5310)

An tSín (GB/YB) SAM (ASTM) an tSeapáin (JIS) An Ghearmáin (DIN GA) Rúis (GOST) ISO
20G 1020 (JIS G3461) STB340 C22 (1.0402), C20C (1.0411) 20 -
20MnG 1022 STB 410 C22 (1.0402) 20Г -
25MnG 1026 STB 510 C26D (1.0415) 25Г -
15MoG ASTM A692 (grád sainithe) (JIS G3462) STBA 12 - - 16Mo3
20MoG ASTM A209 T1a (JIS G3462) STBA13 - - -
12CrMoG ASTM A250 T2 STBA20 - - 13CrMo4-5
15CrMoG ASTM A250 T12 STBA22 - - 13CrMoSi5-5
12Cr2MoG ASTM A250 T22 STBA24 - - 10CrMo9-10
12Cr1MoVG - - - - -
12Cr2MoWVTiB - - - - -
12Cr3MoVSiTiB - - - - 12CrMoV12-10
10Cr9Mo1VNb ASTM A199 T91 STBA26 - - X10CrMoVNb9-1
07Cr18Ni11Nb(1Cr19Ni11Nb roimhe seo) 347H SUS347H X7CrNiNb18-10 (1. 4912) - X7CrNiNb18-10

 

Cuid 3: Steels Dhosmálta le haghaidh Trealamh Brú (GB 13396 Standard)

An tSín (GB/YB) SAM (ASTM) an tSeapáin (JIS) An Eoraip (DIN/BS/NF GA) Rúis (GOST) ISO
06Cr19Ni10(0Cr18Ni9 roimhe seo) A213 TP304 SUS304 X5CrNi18-10 (1. 4301) - X5CrNi18-10
12Cr18Ni9(1Cr18Ni9 roimhe seo) - - X10CrNi18-8 (1. 4310) 12X18H9 X10CrNi18-8
1Cr19Ni9 TP304H SUS304HTB X6CrNi18-10 (1. 4948) - X7CrNi18-9
022Cr19Ni10(00Cr19Ni10 roimhe seo) TP304L SUS304LTB X2CrNi19-11 (1. 4306) 03X18H11 X2CrNi19-11
06Cr18Ni11Ti(0Cr18Ni10Ti roimhe seo) TP321 SUS321TB X6CrNiTi18-10 (1. 4541) 08X18H10T X6CrNiTi18-10
07Cr19Ni11Ti(1Cr18Ni11Ti roimhe seo) TP321H SUS321HTB X6CrNiTi18-10 (1. 4541) 12X18H11T X7CrNiTi18-10
06Cr18Ni11Nb(0Cr18Ni11Nb roimhe seo) TP347 SUS347TB X6CrNiNb18-10 (1. 4550) 08X18H12Б X6CrNiNb18-10
07Cr18Ni11Nb(1Cr19Ni11Nb roimhe seo) TP347H SUS347HTB X7CrNiNb18-10 (1. 4912) - X7CrNiNb18-10
06Cr17Ni12Mo2(0Cr17Ni12Mo2 roimhe seo) TP316 SUS316TB X5CrNiMo17-12-2 (1. 4401) - X5CrNiMo17-12-2
07Cr17Ni12Mo2(1Cr17Ni12Mo2 roimhe seo) TP316H SUS316HTB X3CrNiMo17-13-3 (1. 4436) - -
0Cr18Ni12Mo2Ti TP316Ti SUS316TiTB X6CrNiMoTi17-12-2 (1.4571) - X6CrNiMoTi17-12-2
1Cr18Ni12Mo2Ti TP316Ti SUS316TiTB X6CrNiMoTi17-12-2 (1.4571) - X6CrNiMoTi17-12-2
06Cr17Ni12Mo3Ti(0Cr18Ni12Mo3Ti roimhe seo) TP316Ti SUS316TiTB X6CrNiMoTi17-12-2 (1.4571) 08X17H13M3T X6CrNiMoTi17-12-2
1Cr18Ni12Mo3Ti TP316Ti SUS316TiTB X6CrNiMoTi17-12-2 (1.4571) 08X17H13M3T X6CrNiMoTi17-12-2
1Cr18Ni9Ti TP321 SUS321TB X6CrNiTi18-10 (1. 4541) 12X18H10T X7CrNiTi18-10
06Cr19Ni13Mo3(0Cr19Ni13Mo3 roimhe seo) TP317 SUS317TB - - -
022Cr19Ni13Mo3(00Cr19Ni13Mo3 roimhe seo) TP317L SUS317LTB X2CrNiMo18-15-4 (1.4438) 03X16H15M3 X2CrNiMo 18-15-4 (1.4438)
022Cr19Ni10N(00Cr18Ni10N roimhe seo) TP304LN SUS304LN X2CrNiN18-10 (1. 4311) - X2CrNiN18-9
06Cr19Ni10N(0Cr19Ni9N roimhe seo) TP304N - X5CrNiN19-9 (1. 4315) - X5CrNiN19-9
06Cr23Ni13(0Cr23Ni13 roimhe seo) TP309S SUS309STB X12CrNi23-13 (1. 4833) 10X23H13 X12CrNi23-13
16Cr23Ni13(2Cr23Ni13 roimhe seo) - SUS309TB X15CrNiSi20- 12 (1. 4828) 20X23H12 -

 

Cuid 4: Steels le haghaidh Íseal-Seirbhís Teochta (GB 3531 agus GB/T 18984 Caighdeáin)

An tSín (GB/YB) SAM (ASTM) an tSeapáin (JIS) An Eoraip (DIN/BS/NF GA) Rúis (GOST) ISO
16MnDR A572 Gr. 50 [345] (JIS G3460) STPL380, (JIS G3464) STBL380 E335 (1.0060) 15XCHД E355
15MnNiDR Gr{0}} [345] STPL380, STBL380 E335 (1.0060) 15XCHД E355
09Mn2VDR A572 Gr. 42 [290] STPL 450, STBL 450 E295 (1.0050) 09Г2, 09Г2Д E275
09MnNiDR Gr{0}} [290] STPL 450, STBL 450 E295 (1.0050) 09Г2, 09Г2Д E275
16MnDG Gr{0}} [345] STPL380, STBL380 E335 (1.0060) 15XCHД E355
10MnDG A283 Gr. D (JIS G3101) SS400 S235JR (1. 0038) Ст3кп E235A
09DG Gr. c SS330 - Ст2кп -
09Mn2VDG A572 Gr. 42 [290] (JIS G3460) STPL 450, (JIS G3464) STBL 450 E295 (1.0050) 09Г2, 09Г2Д E275
06Ni3MoDG Gr{0}} [290] STPL 450, STBL 450 E295 (1.0050) 09Г2, 09Г2Д E275