Tugtar carn leatháin chruach Lassen freisin ar U-cineál carn leathán cruach, a bhfuil ról tábhachtach aige mar chineál nua ábhar tógála, maidir le cofferdam droichead, leagan píblíne mór, tochailt díog sealadach chun ithir, uisce agus balla gaineamh a choinneáil; sa caladh, clós díluchtaithe le haghaidh balla coinneála, balla coinneála, cosaint bainc claífoirt, etc., an tionscadal. Tá carn leathán cruach Lassen mar cofferdam, ní hamháin tógáil glas, atá neamhdhíobhálach don chomhshaol agus go tapa, costas tógála íseal, le dea-fheidhm uiscedhíonach.
u cineál bileog méid carn
|
Cineál |
Leithead |
Airde |
Tiús |
Limistéar rannóige |
Meáchan in aghaidh an chairn |
Meáchan in aghaidh an bhalla |
Nóiméad Táimhe |
Modal na rannóige |
|
mm |
mm |
mm |
Cm2/m |
kg/m |
Kg/ m2 |
Cm4/m |
Cm3/m |
|
|
WRU7 |
750 |
320 |
5 |
71.3 |
42.0 |
56.0 |
10725 |
670 |
|
WRU8 |
750 |
320 |
6 |
86.7 |
51.0 |
68.1 |
13169 |
823 |
|
WRU9 |
750 |
320 |
7 |
101.4 |
59.7 |
79.6 |
15251 |
953 |
|
WRU10-450 |
450 |
360 |
8 |
148.6 |
52.5 |
116.7 |
18268 |
1015 |
|
WRU11-450 |
450 |
360 |
9 |
165.9 |
58.6 |
130.2 |
20375 |
1132 |
|
WRU12-450 |
450 |
360 |
10 |
182.9 |
64.7 |
143.8 |
22444 |
1247 |
|
WRU11-575 |
575 |
360 |
8 |
133.8 |
60.4 |
105.1 |
19685 |
1094 |
|
WRU12-575 |
575 |
360 |
9 |
149.5 |
67.5 |
117.4 |
21973 |
1221 |
|
WRU13-575 |
575 |
360 |
10 |
165.0 |
74.5 |
129.5 |
24224 |
1346 |
|
WRU11-600 |
600 |
360 |
8 |
131.4 |
61.9 |
103.2 |
19897 |
1105 |
|
WRU12-600 |
600 |
360 |
9 |
147.3 |
69.5 |
115.8 |
22213 |
1234 |
|
WRU13-600 |
600 |
360 |
10 |
162.4 |
76.5 |
127.5 |
24491 |
1361 |
|
WRU{0}} |
600 |
350 |
12 |
220.3 |
103.8 |
172.9 |
32797 |
1874 |
|
WRU{0}} |
600 |
350 |
13 |
238.5 |
112.3 |
187.2 |
35224 |
2013 |
|
WRU16 |
650 |
480 |
8. |
138.5 |
71.3 |
109.6 |
39864 |
1661 |
|
WRU 18 |
650 |
480 |
9 |
156.1 |
79.5 |
122.3 |
44521 |
1855 |
|
WRU20 |
650 |
540 |
8 |
153.7 |
78.1 |
120.2 |
56002 |
2074 |
|
WRU23 |
650 |
540 |
9 |
169.4 |
87.3 |
133.0 |
61084 |
2318 |
|
WRU26 |
650 |
540 |
10 |
187.4 |
96.2 |
146.9 |
69093 |
2559 |
|
WRU30-700 |
700 |
558 |
11 |
217.1 |
119.3 |
170.5 |
83139 |
2980 |
|
WRU32-700 |
700 |
560 |
12 |
236.2 |
129.8 |
185.4 |
90880 |
3246 |
|
WRU35-700 |
700 |
562 |
13 |
255.1 |
140.2 |
200.3 |
98652 |
3511 |
|
WRU36-700 |
700 |
558 |
14 |
284.3 |
156.2 |
223.2 |
102145 |
3661 |
|
WRU39-700 |
700 |
560 |
15 |
303.8 |
166.9 |
238.5 |
109655 |
3916 |
|
WRU41-700 |
700 |
562 |
16 |
323.1 |
177.6 |
253.7 |
117194 |
4170 |
|
WRU 32 |
750 |
598 |
11 |
215.9 |
127.1 |
169.5 |
97362 |
3265 |
|
WRU 35 |
750 |
600 |
12 |
234.9 |
138.3 |
184.4 |
106416 |
3547 |
|
WRU 38 |
750 |
602 |
13 |
253.7 |
149.4 |
199.2 |
115505 |
3837 |
|
WRU 40 |
750 |
598 |
14 |
282.2 |
166.1 |
221.5 |
119918 |
4011 |
|
WRU 43 |
750 |
600 |
15 |
301.5 |
177.5 |
236.7 |
128724 |
4291 |
|
WRU 45 |
750 |
602 |
16 |
320.8 |
188.9 |
251.8 |
137561 |
4570 |
Buntáistí a bhaineann le carn leatháin chruach U-chruthach
1) Tá sonraíochtaí agus samhlacha saibhir ag U-cineál carn leathán cruach.
2) Deartha agus tháirgtear de réir caighdeán na hEorpa, tá an fhoirm struchtúir siméadrach, atá fabhrach le hathúsáid agus comhionann le rolladh te in athúsáid.
3) Is féidir an fad a shaincheapadh de réir riachtanais na gcustaiméirí, rud a thugann áisiúlacht mhór don tógáil agus laghdaíonn sé an costas ag an am céanna.
4) Mar gheall ar an táirgeadh áisiúil, is féidir é a réamhordú roimh an loingsiú nuair a úsáidtear é i gcomhar le chairn comhcheangailte.
5) Dearadh táirgeachta gearr agus am timthriall, agus is féidir feidhmíocht chairn leatháin chruach a chinneadh de réir riachtanais na gcustaiméirí.
piling cruach Táirgí íomhá

Grianghraf foirne grúpa GNEE

Cuairt chustaiméirí grúpa GNEE

Glacann GNEE Group páirt i dtaispeántas táirgí cruach

Rinneadh tástáil dhian ar chaighdeán ár gcuid táirgí agus tháinig siad le deimhnithe gairmiúla. Má tá aon cheist agat faoi chairn bileog cineál U, bíodh leisce ort iniúchadh a dhéanamh.
Clibeanna Te: u chairn bileog cineál, an tSín u cineál bileog chairn monaróirí, soláthraithe, monarcha