Cainéal C Cruach Iarchurtha Te
Tá cruach cruth C-déanta de phláta te-rollta agus lúbtha fuar. Tá ballaí tanaí aige, meáchan éadrom, airíonna trasghearrtha den scoth agus ard-neart. I gcomparáid le cruach cainéal traidisiúnta, is féidir leis an neart céanna 30% d'ábhair a shábháil.
c cainéal comhdhéanamh ceimiceach miotail
| Eilimint | Céatadán |
| C | 0.26 |
| Cu | 0.2 |
| Fe | 99 |
| Mn | 0.75 |
| P | 0.04 uas |
| S | 0.05 max |
maoin mheicniúil cruach cainéal c
| Impiriúil | méadrach | |
| Dlús | 0.282 lb/in3 | 7.8 g/cc |
| Neart Teanntachta Deiridh | 58,000psi | 400 MPa |
| Neart Teanntachta Táirgeachta | 47,700psi | 315 MPa |
| Neart Fiar | 43,500psi | 300 MPa |
| Leáphointe | 2,590 - 2,670 céim F | 1,420 - 1,460 céim |
| Cruas Brinell | 140 |
| Modh Táirgthe | Te rollta |
c cruach alt méideanna atá ar fáil
| Méid | Doimhneacht | Leithead | Gréasán Tiús |
Fad | Meáchan (lbs/ft) |
| 3" x 3.5# | 3" | 1.35" | .130" | 240.00" | 3.500 |
| 3" x 4.1# | 3" | 1.41" | .170" | 240.00" | 4.100 |
| 3" x 5# | 3" | 1.498" | .258" | 240.00" | 5.000 |
| 3" x 6# | 3" | 1.596" | .356" | 240.00" | 6.000 |
| 4" x 5.4# | 4" | 1.584" | .184" | 240.00" | 5.400 |
| 4" x 6.25# | 4" | 1.647" | .247" | 240.00" | 6.250 |
| 4" x 7.25# | 4" | 1.721" | .321" | 240.00" | 7.250 |
| 5" x 6.7# | 5" | 1.75" | .190" | 240.00" | 6.699 |
| 5" x 9# | 5" | 1.885" | .325" | 240.00" | 9.000 |
| 6" x 8.2# | 6" | 1.92" | .200" | 240.00" | 8.200 |
| 6" x 10.5# | 6" | 2.034" | .314" | 240.00" | 10.500 |
| 6" x 13# | 6" | 2.157" | .437" | 240.00" | 13.000 |
| 7" x 9.8# | 7" | 2.09" | .210" | 240.00" | 9.800 |
| 7" x 12.25# | 7" | 2.194" | .314" | 240.00" | 12.249 |
| 8" x 11.5# | 8" | 2.26" | .220" | 240.00" | 11.500 |
| 8" x 13.75# | 8" | 2.343" | .303" | 240.00" | 13.750 |
| 8" x 18.75# | 8" | 2.527" | .487" | 240.00" | 18.750 |
| 9" x 13.4# | 9" | 2.433" | .230" | 240.00" | 13.400 |
| 9" x 15# | 9" | 2.485" | .285" | 240.00" | 15.000 |
| 10" x 15.3# | 10" | 2.6" | .240" | 240.00" | 15.300 |
| 10" x 20# | 10" | 2.739" | .379" | 240.00" | 20.000 |
| 10" x 25# | 10" | 2.886" | .526" | 240.00" | 24.999 |
| 10" x 30# | 10" | 3.033" | .673" | 240.00" | 30.000 |
| 12" x 20.7# | 12" | 2.94" | .282" | 240.00" | 20.700 |
| 12" x 25# | 12" | 3.047" | .387" | 240.00" | 25.000 |
| 12" x 30# | 12" | 3.17" | .510" | 240.00" | 30.000 |
| 15" x 33.9# | 1.938" | 3" | .400" | 240.00" | 33.900 |
barra cainéal c Táirgí íomhá

Grianghraf foirne grúpa GNEE

Cuairt chustaiméirí grúpa GNEE

Tá go leor Hot Rolled Steel C Channel againn i stoc, agus is féidir linn a shaincheapadh de réir do riachtanas freisin.
Clibeanna Te: te rollta cruach c cainéal, an tSín te rollta cruach c cainéal monaróirí, soláthraithe, monarcha