ASTM A36 ASTM A36/A36M Réamhrá
Grád A36, Cad é Comhdhéanamh CeimiceachASTM A36 ASTM A36/A36M? CeimiceachComhdhéanamh A36 Cruach, airíonna cruach A36, Cruach Carbóin A36, Soláthraí pláta cruach ASTM A36/A36M sa tSeapáin, Bileog cruach ASTM A36/A36M Easpórtálaí, cruach ASTM A36/A36M Praghas, ASTM A36/A36M Cruach comhionann, ASTM A36/A36M cruach soláthróir sa tSín, cruach ASTM A36/A36M grád coibhéiseach Sínis, cruach ASTM A36 ASTM A36/A36M Sonraíochtaí
Feidhmchlár:Cruach struchtúrach carbóin.
Teaschóireáilte:1147 céim - 1419 céim .

Eilimint Cheimiceach ASTM A36 ASTM A36/A36M
Le haghaidh bileog sonraí ASTM A36 ASTM A36/A36M agus comhdhéanamh ceimiceach ASTM A36 ASTM A36/A36M, féach an tábla thíos.
| Eilimint | Min | uas | Cosúil |
|---|---|---|---|
| Cu | 0.2000 | - | - |
| P | - | 0.0400 | - |
| S | - | 0.0500 | - |
| Mn | 0.6000 | 0.9000 | - |
| Si | - | 0.4000 | - |
| C | - | 0.2900 | - |
| Si | - | 0.4000 | - |
| Mn | 0.8500 | 1.3500 | - |
| C | - | 0.2900 | - |

ASTM A36 ASTM A36/A36M Airíonna Meicniúla
| Toradh Rp0.2(MPa) |
Teanntachta Rm(MPa) |
Tionchar KV/Ku (J) |
Fadú A (%) |
Laghdú ar thrasghearradh ar bhriseadh Z (%) |
Coinníoll Mar Teaschóireáilte | Cruas Brinell (HBW) |
|---|---|---|---|---|---|---|
| 222 ( Níos mó ná nó cothrom le ) | 215 ( Níos mó ná nó cothrom le ) | 43 | 44 | 42 | Réiteach agus Aosú, Annealing, Ausaging, Q+T, etc | 341 |
ASTM A36 ASTM A36/A36M Airíonna Fisiceacha
Tugann na liostaí seo a leanas airíonna ASTM A36 ASTM A36/A36M amhail airíonna fisiceacha, dlús, leathnú teirmeach.
| Teocht ( céim ) |
Modal leaisteachas (GPa) |
Meán chomhéifeacht leathnaithe teirmeach 10-6/( céim ) idir 20( céim ) agus | Seoltacht theirmeach (W/m· céim ) |
Cumas teirmeach sonrach (J/kg· céim ) |
Friotaíocht leictreach ar leith (Ω mm²/m) |
Dlús (kg/dm³) |
Comhéifeacht Poisson, ν |
|---|---|---|---|---|---|---|---|
| 41 | - | - | 0.23 | - | |||
| 662 | 898 | - | 14.3 | 222 | - | ||
| 494 | - | 22 | 44.2 | 144 | 213 |