SA 387 Grád 11 Rang 2 is pláta cruach cóimhiotal moile ASME/ASTM é do shoithí brú ardteochta, comhionann leASTM A387 grád 11 rang 2 saor in aisce, a bhfuil airíonna comhchosúla le fáil freisin iBS 621B; tá sé sainmhínithe ag a chomhdhéanamh ceimiceach (thart ar 1.25% Cr, 0.50% Mo) agus airíonna meicniúla sonracha cosúil le neart teanntachta níos airde (515-690 MPa) i gcomparáid le hAicme 1, ag tairiscint friotaíocht ocsaídiúcháin / creimthe níos fearr d'iarratais éilitheacha.

Tábla Comparáide Thapa Coibhéise
| Caighdeán | Grád Coibhéiseach | Nótaí |
|---|---|---|
| ASME | SA 387 Gr 11 Cl.2 | 1.25Cr-0.5Mo, N+T |
| ASTM | A387 Gr 11 Cl.2 | Cúpla ábhar |
| GA | 13CrMo4-5 (1.7335) | An choibhéis AE is gaire |
| DIN | 13CrMo4-5 | Fealsúnacht cheimic chéanna |
| GB | 12Cr1MoVR | Cruach soitheach brú |
| JIS | SCMV2 | Teas{0}}Cr-Mo cruach atá frithsheasmhach ó thaobh teasa |
| BS | 1501-621-440B | Coibhéis oidhreachta |
SA387 Gr.11 CL.2Cumadóireacht Cheimiceach
|
SA387 Gr.11 CL.2Comhdhéanamh Ceimiceach |
|||||||
|
Grád |
An Eilimint Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Cr |
Mo |
|
|
SA387 Gr.11 Cl.2 |
0.04-0.17 |
0.44-0.86 |
0.35-0.73 |
0.035 |
0.035 |
0.94-1.56 |
0.40-0.70 |
SA387 Gr.11 CL.2 Maoin Mheicniúil
|
Grád |
SA387 Gr.11 CL.2Maoin Mheicniúil |
|||
|
Tiús |
Toradh |
Teanntachta |
Fadú |
|
|
SA387 Gr.11 Cl.2 |
mm |
Mpa is lú |
Mpa |
íosmhéid % |
|
t Níos lú ná nó cothrom le 50 |
310 |
515-690 |
18 |
|
|
50<> |
- |
- |
- |
|

Feidhmchláir tipiciúla
Sliogáin & cinn soitheach brú
Malartóirí teasa bhlaosc & feadán
Imoibreoirí agus deighilteoirí
Coirí agus drumaí gaile
Trealamh scaglainne agus peitriceimiceach
Bí i dteagmháil le GNEE inniuchun do riachtanais choibhéiseacha SA 387 Gr 11 Aicme 2 a phlé agus plátaí cruach ardchaighdeáin a fháil do do threalamh tionsclaíoch!
Cad é coibhéis 387 gr 11 cl 2 leis?
ASME SA387
Is é Sa 387 Gr 11 Ábhar Coibhéiseach an ASME SA387 i margaí na SA agus tá modúil ag an Aontas Eorpach i ngrád 13CrMoSi5-5. Is é an Sa 387 Gr 11 Cl 2 Ábhar Coibhéiseach anSA387-11-2den chaighdeán ASME agus ASTM.
Cad é an difríocht idir SA 387 Grád 11 CL 1 agus Rang 2?
Tá an difríocht idir SA 387 Grád 11 Aicme 1 agus Pláta Aicme 2 ina n-airíonna meicniúla. Mar sin féin, tá an comhdhéanamh ceimiceach céanna acu araon.Tá neart teanntachta agus neart toraidh ábhar rang 2 níos airde ná rang 1, ach tá fadú rang 1 níos airde i gcomparáid le rang 2.
Cad é atá comhionann le SA 387?
Cad é ábhar coibhéiseach SA 387? Is iad na hábhair Choibhéiseacha de Sa 387 Gr 12BS 620B, UNS K11757, A387 / SA 387, DIN 13 CRMO 44, agus EN 3 CRMO 45
Cad é ábhar coibhéiseach SA 387 GR 12 Cl 2?
Is iad na hábhair Choibhéiseacha de Sa 387 Gr 12BS 620B, UNS K11757, A387 / SA 387, DIN 13 CRMO 44, agus EN 3 CRMO 45.
Cad é an choibhéis ASTM A387 Grád 22 ?
I measc na ngrád cruach coibhéiseach ASTM A387 Grád 22,SA387 Grád 22, 10CrMo9-10Tá níos mó tóir ná a gcomhionann eile. Tá cruach SA387 Grád 22 faoi chaighdeán ASME SA387/ SA387M. Tá feidhmíocht cheimiceach agus ceanglais theicniúla cruach SA387 Grád 22 beagnach mar an gcéanna le cruach ASTM A387 Grád 22.
Taispeáin Táirgí



Pacáil & Loingseoireacht


Taispeántais agus Cuairteanna Custaiméirí

Soláthraíonn GNEE Steel éagsúlacht de choirí agus plátaí cruach soithí brú, mar shampla A204 Grád B, A515 Grád 70, A537 Aicme 1, SA387 Grád 11 Aicme 1, P265GH, S537 Aicme 2, P355Q, P275N, P355N, P695Q, etc. is féidir glaoch ar bheolíne an chomhairliúcháin ag +8615824687445 nó ríomhphost a sheoladh chuig alloy@gneesteelgroup.com. Tá fáilte romhat dul i gcomhairle linn, agus táimid an-sásta do cheisteanna a fhreagairt.
| Gráid Phlátaí Árthaí Brú arna Sholáthar ag GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Grád A | ASTM A202 Grád B | ||
| ASTM A203/A203M | ASTM A203 Grád A | ASTM A203 grád B | ASTM A203 Grád D | ASTM A203 Grád E | |
| ASTM A203 Grád F | |||||
| ASTM A204/A204M | ASTM A204 Grád A | ASTM A204 grád B | ASTM A204 Grád C | ||
| ASTM A285/A285M | ASTM A285 Grád A | ASTM A285 Grád B | ASTM A285 Grád C | ||
| ASTM A299/A299M | ASTM A299 Grád A | ASTM A299 grád B | |||
| ASTM A302/A302M | ASTM A302 Grád A | ASTM A302 grád B | ASTM A302 Grád C | ASTM A302 Grád D | |
| ASTM A387/A387M | ASTM A387 grád 5 rang 1 saor in aisce, | ASTM A387 grád 5 rang 2 saor in aisce | ASTM A387 grád 11 rang 1 saor in aisce, | ASTM A387 grád 11 rang 2 saor in aisce | |
| ASTM A387 rang 12 saor in aisce, | ASTM A387 grád 12 rang 2 saor in aisce | ASTM A387 grád 22 rang 1 saor in aisce, | ASTM A387 grád 22 rang 2 saor in aisce | ||
| ASTM A515/A515M | ASTM A515 Grád 60 saor in aisce, | ASTM A515 grád 65 | ASTM A515 grád 70 | ||
| ASTM A516/A516M | ASTM A516 grád 55 | ASTM A516 Grád 60 saor in aisce, | ASTM A516 grád 65 | ASTM A516 grád 70 | |
| ASTM A517/A517M | ASTM A517 Grád A | ASTM A517 Grád B | ASTM A517 Grád E | ASTM A517 Grád F | |
| ASTM A517 Grád P | ASTM A517 Grád J | ||||
| ASTM A533/A533M | ASTM A533 Grád A Aicme 1 | ASTM A533 Grád B Aicme 1 | ASTM A533 Grád C Rang 1 | ASTM A533 Grád D Rang 1 | |
| ASTM A533 Grád A Rang 2 | ASTM A533 Grád B Rang 2 | ASTM A533 Grád C Rang 2 | ASTM A533 Grád D Rang 2 | ||
| ASTM A533 Grád A Aicme 3 | ASTM A533 Grád B Rang 3 | ASTM A533 Grád C Rang 3 | ASTM A533 Grád D Rang 3 | ||
| ASTM A537/A537M | ASTM A537 Aicme 1 | ASTM A537 Aicme 2 | ASTM A537 Aicme 3 | ||
| ASTM A612/A612M | Tiománaí ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Grád A | ASTM A662 Grád B | ASTM A662 Grád C | ||
| GA | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| GA10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB{0}}CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | Din 17155 HÉ | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||