Pláta cruach teorollta A203 GrBle neart toraidh íosta ag 275 Mpa, níos airde ná pláta cruach soithigh brú A203 Grád A ag 255 Mpa, agus beidh an neart teanntachta os cionn 480 Mpa do phláta cruach SA203 Grád B.
Maoin mheicniúil le haghaidh pláta cruach A203 Grád B
| Neart toraidh (Níos mó ná nó cothrom le Mpa) | Neart teanntachta (Mpa) | Fadú ar mó é ná nó cothrom le , % | |
| 275 | 485-620 | 200mm | 50mm |
| 17 | 21 | ||
Comhdhéanamh ceimiceach do phláta cruach A203 Grád B (Anailís Teasa Max%)
| Comhdhéanamh príomh-eilimintí ceimiceacha pláta cruach A203 Grád B | ||||||
| Tiús(mm) | C | Si | Mn | P | S | Ni |
| T Níos lú ná nó cothrom le 50 | 0.21 | 0.15-0.40 | 0.70 | 0.035 | 0.035 | 2.10-2.50 |
| 50<> | 0.24 | 0.80 | ||||
Riachtanais Theicniúla & Seirbhísí Breise le haghaidh pláta cruach cóimhiotal nicile A203GRB
Tástáil teannas ard
Tástáil tionchar teocht íseal
Postáil insamhladh-chóireáil teasa táthaithe (PWHT)
Rollta faoi chaighdeán NACE MR-0175 (HIC+SSCC)
Teastas tástála Muileann Bunúsaigh eisithe faoi EN 10204 FORMÁID 3.1/3.2
Pléascadh lámhaigh agus Péinteáil, Gearradh agus táthú de réir éilimh an úsáideora deiridh
Tástáil Tionchair Teocht Íseal
Chun meastóireacht a dhéanamh ar fheidhmíocht plátaí cruach ASTM A203/A203M A203 Grád B(A203GrB) le haghaidh soithí brú ag teocht íseal, tá gá le tástáil tionchair íseal-teocht. Is féidir leis an tástáil seo cruas agus friotaíocht briste cruach atá faoi réir tionchair ag teochtaí ísle a thástáil. A203/A203M A203 Grád B(A203GrB) Ní mór do phlátaí cruach le haghaidh soithí brú pas a fháil i dtástáil tionchair ísealteochta lena chinntiú go bhfuil siad sábháilte agus iontaofa le húsáid i dtimpeallachtaí ísealteochta.
Príomhchásanna Iarratais dePláta cruach coire rollta te ASTM A203 Grád B
Tionscal Peitriceimiceach
ASTM A203 grád BÚsáidtear Plátaí Cruach Árthaí Brú go forleathan sa tionscal peitriceimiceach, go príomha le haghaidh déantúsaíochta trealaimh ar nós imoibreoirí, malartóirí teasa, agus deighilteoirí. Tá na trealamh seo faoi réir teocht ard, brú ard, agus creimeadh ó mheáin éagsúla le linn an phróisis táirgthe peitriceimiceach. Mar gheall ar ard-neart agus friotaíocht creimeadh plátaí cruach SB480, tá siad in ann na coinníollacha oibriúcháin déine seo a chomhlíonadh.
Tionscal Ceimiceach
Sa tionscal ceimiceach,ASTM A203 grád BÚsáidtear -Plátaí Cruach Coire ar ardchaighdeán chun coimeádáin agus píblínte éagsúla a dhéanamh. Ní mór do na coimeádáin agus na píblínte seo creimeadh agus creimeadh ó mheáin cheimiceacha éagsúla a sheasamh, agus cinntíonn ard-neart agus friotaíocht scríobadh plátaí cruach SB480 oibriú cobhsaí fadtéarmach an trealaimh.
Stáisiúin Cumhachta agus Coirí
ASTM A203 grád BTá feidhmeanna forleathana ag plátaí teorollta i dtionscail na stáisiún cumhachta agus na gcoire. Úsáidtear iad chun trealamh a dhéanamh ar nós drumaí gaile coire, píopaí uisce ardbhrú do stáisiúin hidreachumhachta, agus toirteanna tuirbíní. Tá na trealamh seo faoi réir teocht ard agus ardbhrú gaile agus creimeadh uisce le linn oibriú stáisiúin chumhachta agus coirí, agus tá ard-neart agus friotaíocht tuirse agASTM A203 grád Bcinntíonn plátaí cruach cóimhiotail nicil iontaofacht agus sábháilteacht an trealaimh.
Réimsí Eile
Seachas na-réimsí thuasluaite,ASTM A203 grád BIs féidir Plátaí Cruach Coire agus Soithí Brú a úsáid freisin chun coimeádáin táthaithe singil-chiseal, coimeádáin táthaithe ilchiseal{- muinchille te, coimeádáin fillte ilchiseal, agus coimeádáin aicme eile den dara agus den tríú{5} chomh maith le soithí brú ísealteochta. Ina theannta sin, is féidir iad a úsáid chun trealamh stórála a mhonarú cosúil le sorcóirí gáis peitriliam leachtaithe.
Más mian leat tuilleadh a fhoghlaim faoi tháirgí GNEE, is féidir leat ríomhphost a sheoladh chuigalloy@gneesteelgroup.com. Táimid thar a bheith sásta cabhrú leat.
| Gráid Phlátaí Árthaí Brú arna Sholáthar ag GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Grád A | ASTM A202 Grád B | ||
| ASTM A203/A203M | ASTM A203 Grád A | ASTM A203 grád B | ASTM A203 Grád D | ASTM A203 Grád E | |
| ASTM A203 Grád F | |||||
| ASTM A204/A204M | ASTM A204 Grád A | ASTM A204 grád B | ASTM A204 Grád C | ||
| ASTM A285/A285M | ASTM A285 Grád A | ASTM A285 Grád B | ASTM A285 Grád C | ||
| ASTM A299/A299M | ASTM A299 Grád A | ASTM A299 grád B | |||
| ASTM A302/A302M | ASTM A302 Grád A | ASTM A302 grád B | ASTM A302 Grád C | ASTM A302 Grád D | |
| ASTM A387/A387M | ASTM A387 grád 5 rang 1 saor in aisce, | ASTM A387 grád 5 rang 2 saor in aisce | ASTM A387 grád 11 rang 1 saor in aisce, | ASTM A387 grád 11 rang 2 saor in aisce | |
| ASTM A387 rang 12 saor in aisce, | ASTM A387 grád 12 rang 2 saor in aisce | ASTM A387 grád 22 rang 1 saor in aisce, | ASTM A387 grád 22 rang 2 saor in aisce | ||
| ASTM A515/A515M | ASTM A515 Grád 60 saor in aisce, | ASTM A515 grád 65 | ASTM A515 grád 70 | ||
| ASTM A516/A516M | ASTM A516 grád 55 | ASTM A516 Grád 60 saor in aisce, | ASTM A516 grád 65 | ASTM A516 grád 70 | |
| ASTM A517/A517M | ASTM A517 Grád A | ASTM A517 Grád B | ASTM A517 Grád E | ASTM A517 Grád F | |
| ASTM A517 Grád P | ASTM A517 Grád J | ||||
| ASTM A533/A533M | ASTM A533 Grád A Aicme 1 | ASTM A533 Grád B Aicme 1 | ASTM A533 Grád C Rang 1 | ASTM A533 Grád D Rang 1 | |
| ASTM A533 Grád A Rang 2 | ASTM A533 Grád B Rang 2 | ASTM A533 Grád C Rang 2 | ASTM A533 Grád D Rang 2 | ||
| ASTM A533 Grád A Aicme 3 | ASTM A533 Grád B Rang 3 | ASTM A533 Grád C Rang 3 | ASTM A533 Grád D Rang 3 | ||
| ASTM A537/A537M | ASTM A537 Aicme 1 | ASTM A537 Aicme 2 | ASTM A537 Aicme 3 | ||
| ASTM A612/A612M | Tiománaí ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Grád A | ASTM A662 Grád B | ASTM A662 Grád C | ||
| GA | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| GA10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB{0}}CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | Din 17155 HÉ | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||