JFE{0}}EH360 Pláta Frithsheasmhach in aghaidh Scríoblach
JFE{0}EH360 Cruach resistant caitheamh Seapánach, JFE Is é EH360 pláta cruach resistant caitheamh na Seapáine JFE Steel, agus gráid eile JFE{6}EH400, JFE{8}EH500, JFE Steel Is é an chéad cheann a tháirgeann agus a dhíol an pláta cruach atá resistant a chaitheamh ó thús an dara leath, ó thús an dara leath den chruach. a úsáidtear go forleathan mar ábhar tábhachtach le haghaidh innealra tógála, innealra mianadóireachta, agus innealra talmhaíochta.
Sraith ar Fáil ó Phlátaí Caith JFE-EH360
| Cruas dromchla Brinell [ráthaithe] |
Ainm branda | Tiús(mm) | Cineál | Airíonna tionchair charpy | |
|---|---|---|---|---|---|
| Fuinneamh súite carpy(J) [ráthaithe] |
Tástáil teocht ( céim ) |
||||
| 500±40 | EVERHARD-C500 | 5〜101.6 | Caighdeán Sraith |
ーーー | ーーー |
| 400±30 | EVERHARD-C400 | 5〜101.6 | |||
| 550±40 | EVERHARD-C550 | 5〜32 | |||
| 340±30 | EVERHARD-C340 | 38〜160 | |||
| 450±25 | EVERHARD-C450 | 5〜101.6 | |||
| Níos mó ná 401 nó cothrom leis | EVERHARD-SP | 5〜65 | Grád Sár | ーーー | ーーー |
| 450±25 | EVERHARD-C450LE | 5〜50.8 | Sraith Ard-Thoughness | Níos mó ná nó cothrom le 27 | -40 |
| 400±30 | EVERHARD-C400LE | 5〜60 | Níos mó ná nó cothrom le 27 | -40 | |
| 500±40 | EVERHARD-C500LE | 5〜50.8 | Níos mó ná nó cothrom le 27 | -40 | |
JFE -Méid pláta cruach scríobadh EH360
| Leithead (mm) | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| 2401 ~2600 |
1801 ~2000 |
1501 ~ 1800 |
2201 ~2400 |
2801 ~ 3000 |
2001 ~2200 |
3001 ~ 3200 |
3201 ~3400 |
3401 ~3600 |
||
| T h i c k n e s s (mm) |
22.1~24.0 | 18 | 22 | 24 | 20 | 14 | 22 | 12 | - | - |
| 10.0~11.9 | 14 | 20 | 22 | 16 | 12 | 18 | - | - | - | |
| 14.0~22.0 | 14 | 20 | 22 | 16 | 12 | 18 | - | - | - | |
| 12.0~12.9 | 14 | 20 | 22 | 16 | 12 | 18 | - | - | - | |
| 9.0~9.9 | 12 | 16 | 18 | 12 | - | 14 | - | - | - | |
| 13.0~13.9 | 14 | 20 | 22 | 16 | 12 | 18 | - | - | - | |
| 26.1~28.0 | 22 | 25 | 25 | 24 | 20 | 24 | 18 | 16 | 14 | |
| 30.1~35.0 | 25 | 25 | 25 | 25 | 24 | 25 | 22 | 22 | 22 | |
| 24.1~26.0 | 20 | 24 | 25 | 22 | 16 | 22 | 14 | 12 | - | |
| 40.1~45.0 | 25 | 25 | 25 | 25 | 25 | 25 | 25 | 24 | 23 | |
| 28.1~30.0 | 25 | 25 | 25 | 25 | 22 | 25 | 20 | 20 | 18 | |
| 50.9~60.0 | 24 | 23 | 25 | 21 | 20 | 23 | 19 | 18 | 17 | |
| 35.1~40.0 | 25 | 25 | 25 | 25 | 25 | 25 | 24 | 22 | 22 | |
| 70.1~80.0 | 18 | 17 | 19 | 16 | 15 | 17 | 14 | 13 | 13 | |
| 45.1~50.8 | 25 | 25 | 25 | 25 | 25 | 25 | 23 | 22 | 20 | |
| 80.1~90.0 | 16 | 15 | 17 | 14 | 13 | 15 | 13 | 12 | 11 | |
| 60.1~70.0 | 20 | 19 | 22 | 18 | 17 | 20 | 16 | 15 | 14 | |
| 90.1~100.0 | 14 | 13 | 15 | 12 | 12 | 14 | 11 | 10 | 10 | |
Feidhmchlár táirgí cruach pláta caithimh JFE-EH360
JFE - EH360 Pláta Cruach Seapánach Frithsheasmhach in aghaidh Caithimh:Is féidir é a úsáid chun trealamh ardchaighdeáin agus páirteanna spártha a mhonarú agus a shaol seirbhíse a mhéadú, an baol do chliseadh a laghdú agus mar sin an cumas táirgthe a mhéadú. linings.JFE-H360 Wear Resistant Steel Plate is féidir a sheasamh de chineál ar bith abrasion agus caitheamh ó gach cineál carraige, gaineamh agus scríobadh gairbhéil .
JFE{0}}EH360 Caith pláta cruach Íomhá Táirgí

Grianghraf foirne grúpa GNEE

Cuairt chustaiméirí grúpa GNEE

Tá seirbhís tar éis díolacháin den scoth againn. Má tá aon cheist agat faoi JFE- EH360 Abrasion Resistant Plate, is féidir leat teagmháil a dhéanamh linn agus cuirfimid freagra chugat laistigh de dhá uair an chloig.